Indexed by:
Abstract:
A sinter's density, porosity and equivalent thermal conductivity were measured. The variation of equivalent thermal conductivity with temperature was studied. The results showed that equivalent thermal conductivity increased with temperature during 323~750 K and reached a peak near 750 K. After the temperature rised above 750 K, part of sinter melted with equivalent thermal conductivity reduced. The temperature of sinter at actual cooling process was below 723 K. Simulated results showed that with the rising of temperature solid thermal conductivity increased linearly from 323 K to 723 K, Numerical simulation of equivalent thermal conductivity validated by experimental measurement were better than the experience value. © 2017, Science Press. All right reserved.
Keyword:
Reprint Author's Address:
Email:
Source :
The Chinese Journal of Process Engineering
ISSN: 1009-606X
Year: 2017
Issue: 4
Volume: 17
Page: 879-882
Cited Count:
WoS CC Cited Count: 0
SCOPUS Cited Count: 2
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 8
Affiliated Colleges: