Indexed by:
Abstract:
In this paper, deformation and stress of casting shell and the resin prototype pattern are analyzed, getting the criterion of non-crack. And solid prototype pattern which is in the diameter of 30mm and hollow prototype pattern which is in the diameter of 30mm with thickness of 1mm are prepared, then coated and sanded, baked to get the casting shell. The results show that criterion of non-crack of casting shell is based on cross sectional ratio M of casting shell, and hollow prototype pattern is more reasonable. When charging temperature is 80 to 100 degrees C, heating rate is 150 degrees C/h, the prototype pattern is heated to 950 degrees C for 30min, then the integrated casting shell is obtained.
Keyword:
Reprint Author's Address:
Email:
Source :
OPTOELECTRONICS AND ADVANCED MATERIALS-RAPID COMMUNICATIONS
ISSN: 1842-6573
Year: 2016
Issue: 1-2
Volume: 10
Page: 91-96
0 . 5 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
ESI HC Threshold:305
CAS Journal Grade:4
Cited Count:
WoS CC Cited Count: 1
SCOPUS Cited Count:
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 7
Affiliated Colleges: