Abstract:
介绍了2524与7150铝合金激光焊T型接头优化的工艺参数,并研究了T型接头在优化工艺下的显微组织与力学性能,进行金相分析、显微硬度测试与接头拉伸试验.结果表明:优化工艺下焊缝没有裂纹、气孔,金相组织晶粒细小、致密,焊缝区域的硬度最低;T型接头x方向的拉伸强度达到384 MPa,z方向的拉伸强度为236 MPa.