以低熔点盐为原料,通过熔盐法及煅烧合成纳米富锂正极材料Li12 Ni0.2 Mn0.6 O2.煅烧温度对产物的结构、形貌和电化学性能有直接影响.在800℃烧结10 h可得到粒径均一、层状结构良好、具有良好循环性能和较高倍率性能的纳米富锂材料.在2.0~4.8 V以1.0 C(200mA/g)倍率充放电,首次放电比容量为185 mAh/g,循环50次的容量保持率为94%.