采用不同的方法制备出四种不同形貌的MnCO3作为前驱体,在H2/Ar混合气氛中热处理合成出规则的球形、立方体、哑铃体、椭球形四种不同形貌的MnO微/纳米材料.采用XRD、SEM、TG等方法对材料的结构和形貌进行表征.采用恒电流充放电方法比较了四种形貌的MnO材料用作锂离子电池负极材料时电化学性能.结果表明:0.1 C充放电时,球形和立方体形貌的MnO材料比容量较高,20次循环后保持在250 mAh/g以上.