研究铸造及挤压Mg-12Zn-1.5Er合金的显微组织及力学性能。结果表明:铸造Mg-12Zn-1.5Er合金中的I相在挤压过程中被破碎,并且动态再结晶伴随着挤压过程发生,导致合金组织进一步细化。合金的晶粒为等轴晶,其平均晶粒尺寸为25μm;并且观察到大量的纳米级颗粒在动态再结晶晶粒中析出;与铸造合金相比,挤压合金的力学性能明显提高,这是因为组织细化、准晶强化及纳米级颗粒的析出强化;挤压合金的抗拉强度、屈服强度分别为359MPa和318MPa。