以L-半胱氨酸为硫源,明胶作为组装剂.采用水热方法制备了粒径均一的ZnS微米球.利用XRD,TEM,FESEM,FTIR探讨了明胶、反应时间和反应温度对产物形貌和尺寸的影响,其结果表明ZnS微米球是由ZnS纳米颗粒组装而成的3D多级结构.光催化性能研究表明,明胶的加入提高了最终产物的光催化性能.利用产物的荧光发光性能解释了其光催化性能产生差异的因为.