Zeolite P was synthesized for the first time via a novel water-bathing route at 90 C using scrubbed diatomite, sodium hydroxide, and aluminum hydroxide as precursor, with SiO2/Al2O3, SiO2/Na2O, and H2O/Na2O molar ratios of 7.43, 3.81, and 80.00, respectively. The as-fabricated samples were characterized by means of scanning electron microscopy. X-ray diffraction, and nitrogen adsorption measurements. This study showed that (i) treating the diatomite raw material with sodium hexametaphosphate could open the pores in the diatomite via removal of the clay clogged in its pores; (ii) tetragonal mesoporous zeolite P samples with a surface area of 56-60 m(2)/g could be generated after 6-24 h of water-bathing reaction at 90 degrees C; (iii) extension of water-bathing reaction time could improve the mesoporous structure of zeolite P; and (iv) Ca2+ adsorption capacity of the zeolite P sample was about 300 cmol/kg. Such high-surface-area porous zeolite P could be used as an effective adsorbent for the treatment of water containing calcium and magnesium ions. (C) 2010 Chinese Society of Particuology and Institute of Process Engineering, Chinese Academy of Sciences. Published by Elsevier B.V. All rights reserved.
Keyword:
Reprint Author's Address:
Email:
Source :
PARTICUOLOGY
ISSN: 1674-2001
Year: 2011
Issue: 2
Volume: 9
Page: 174-178
3 . 5 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
JCR Journal Grade:2
CAS Journal Grade:3
Cited Count:
WoS CC Cited Count: 46
SCOPUS Cited Count: 46
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 5