Abstract:
当高铬白口铸铁含铬量为18%~28%,Cr/C值是8~9,铸铁的显微组织是回火马氏体+少量残余奥氏体(<5%)+M7C3碳化物,则磨球具有高的冲击韧性和断裂韧性KIC,具有高的冲击抗力,表现出低的冲击剥落量.