Scandia and rhenium doped tungsten powders were prepared by solid-liquid doping combined with two-step reduction method. The particle size of doped tungsten and distribution of scandia and rhenium were studied by SEM, EDS, XRD and granularity analysis. Experimental results showed that scandia distributed evenly on the surface of tungsten particles. Addition of scandia and rhenium decreased the particle size of doped tungsten, and the more the content of scandia and rhenium, the smaller the doped tungsten particles. Tungsten powders doped with 3 % Sc2O3 and 3 % Re (mass fraction) had an average size of about 80 nm in diameter. The mechanism of the decrease in the tungsten particle size was discussed.
Keyword:
Reprint Author's Address:
Email:
Source :
JOURNAL OF RARE EARTHS
ISSN: 1002-0721
Year: 2007
Issue: 2
Volume: 25
Page: 194-198
4 . 9 0 0
JCR@2022
ESI Discipline: CHEMISTRY;
JCR Journal Grade:4
Cited Count:
WoS CC Cited Count: 14
SCOPUS Cited Count: 14
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 7
Affiliated Colleges: