Abstract:
研究了等温温度、保温时间和变形量对Mg-6Al-0.9Er合金组织与性能的影响,并对比分析了等温热处理前后Mg-6Al-xEr的拉伸和冲击性能。结果表明,不同等温温度下Mg-6Al-0.9Er合金的组织都由白色基体α-Mg和灰黑色β-Mg_(17)Al_(12)相组成,随着等温温度的升高,α-Mg枝晶逐渐转变为球晶,圆整度提高、晶粒变小,Mg-6Al-0.9Er合金的显微硬度呈现逐渐升高的趋势;随着等温时间的延长,Mg-6Al-0.9Er合金的晶粒逐渐圆整和细化,并在等温时间为15min时形成了完整等轴晶,显微硬度呈现逐渐升高的趋势;随着压缩变形量的增加,合金晶粒趋于圆整化,Mg-6Al-0....