Abstract:
采用紫外-臭氧(UVO)辐照方式对挤塑聚苯乙烯保温板(XPSF)进行了表面改性,通过X射线光电子能谱仪(XPS)、接触角测量仪(CA)和扫描电子显微镜(SEM)对改性前后XPSF表面化学结构、润湿性能及表面形貌的变化规律进行了表征和测试。结果表明,随着UVO辐照时间的延长,XPSF表面含氧官能团数量逐渐增加,尤其在15 min时,XPSF表面的O/C值(O和C原子含量比值)由0.04增加至0.59;经UVO辐照30 min后,XPSF表面与水的接触角从未经处理的101.7°降至37.1°;UVO辐照前后XPSF表面形貌差异很小;随着放置时间的延长,XPSF表面氧含量逐渐降低,表面形成的含氧官能...