一种掺杂炭化ZIF‑8多孔材料的铅炭电池正极的制备方法,属于铅炭电池正极材料技术领域。将具有高比表面积、高导电性、高电容和有序分布的孔结构的炭化ZIF‑8材料掺于铅炭电池正极时,不仅提高了铅炭电池的充电接受能力和循环性能,且提高了电解液向正极活性物质的扩散量和均匀性,抑制了电池的PCL(早期容量损失)现象,有效提高了铅炭电池的整体性能。
Keyword:
Reprint Author's Address:
Email:
Patent Info :
Type: 发明申请
Patent No.: CN201710764824.X
Filing Date: 2017-08-30
Publication Date: 2018-01-19
Pub. No.: CN107611387A
Applicants: 北京工业大学
Legal Status: 驳回