Indexed by:
Abstract:
一种柔性电磁屏蔽材料的制备方法,属于电磁屏蔽材料的制备技术,它包括以下各步骤,即材料经超声及碱性液予处理,水洗后基材放入酸性粗化液中粗化处理,予处理液中活化予处理,活化液中活化处理,还原液中还原处理,沉铜液中沉铜处理,沉镍合金液中电镀镍合金、沉镍合金混合处理,及材料水洗后浸入电镀镍合金液中的电镀镍合金处理。该方法制成的材料具有屏蔽体分布均匀,屏蔽层厚度小于1微米,柔韧性好,综合屏蔽效能持久等特点。
Keyword:
Reprint Author's Address:
Email:
Patent Info :
Type: 发明授权
Patent No.: CN00132720.8
Filing Date: 2000-11-16
Publication Date: 2003-09-03
Pub. No.: CN1120654C
Applicants: 北京工业大学
Legal Status: 期限届满
Cited Count:
WoS CC Cited Count: 0
SCOPUS Cited Count:
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 6