The potential of using waste glass powder to increase the chloride binding capacity of fly ash/cement hardened paste was investigated. When only fly ash replacing cement, the chloride binding capacity was raised within 28d when the fly ash replacement level was in the range from 30-50% by mass. But at a longer age of 60 to 90d, the binding performance was increased at the replacement level of 10-30wt%. The chloride binding capacity of glass powder-fly ash-cement system was increased by adding glass powder of 2% and 4% by mass at 7d while those at larger addition and longer age reduced. The reduction was found to be related to the release of alkali ion due to the addition of glass powder in the paste. © ICDCS 2018. All rights reserved.
Keyword:
Reprint Author's Address:
Email:
Source :
Year: 2018
Page: 290-294
Language: English
Cited Count:
WoS CC Cited Count: 0
SCOPUS Cited Count:
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 9
Affiliated Colleges: