The Intergranular Corrosion (IGC) properties of Al-xMg-0.6Mn(x=3, 4, 5, 6 and 7)wt.% alloys were studied using the mass loss test. The mass loss test results of the alloys annealed at 100-300°C for 1h indicated that the alloys with 3 and 4% Mg were resistant to IGC. While the mass loss values of the 6 and 7% Mg alloys were increased to IGC severe sensitive region, and then abruptly fallen to the IGC-resistant region with the increasing temperature. The mass loss-temperature curve of 5% Mg alloy was actually located between them. After isothermal annealing, the mass loss results indicated a stabilization temperature of the alloys with 5, 6 and 7% Mg appeared at the temperature beyond 220°C, 250°C and 270°C, respectively. Furthermore, below the stabilization temperature 10-20°C, it was observed a type of 'special mass loss curve ' in so-called transition region that was showed a quick mass loss increasing to sensitization region and then a decrease to the IGC resistant region with a prolonged annealing time. To explore the 'special curve' in transition region, the TEM observation of Al-7Mg alloy annealing at 250°C was conducted, which indicated the sensitization resulted from the continuity of β phase, while the descending to the IGC might to be attributed to the spheroidization of β phase. © 2017 Trans Tech Publications, Switzerland.
Keyword:
Reprint Author's Address:
Email:
Source :
ISSN: 0255-5476
Year: 2017
Volume: 877
Page: 514-521
Language: English
Cited Count:
WoS CC Cited Count: 0
SCOPUS Cited Count: 12
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 3
Affiliated Colleges: