Abstract:

This paper presents the morphology evolution of the interfacial intermetallic compound (IMC) in Cu/Sn-58Bi/Cu solder joint during current stressing and loading temperatures. The IMC growth kinetics and Bi migration towards the anode side was analyzed and discussed. One dimensional semicircular sectioned solder joint was fabricated and used to conduct the electromigration (EM) experiment, effectively eliminated the thermomigration effect induced by Joule heating accumulation. Results indicated that the solder matrix was melted due to the combined effect of electromigration force and high temperature. After cutting off the circuit, huge valleys were found in the solder joints. Furthermore, partial bulk solder extended upon the Cu substrates. For further detecting the microstructural evolution of the solder matrix, the tested sample was polished to reveal the interior microstructure. It can be noted that the eutectic microstructure coarsened slightly, but remained the original uniform distribution. Most important, the IMC layer formed at the anode interface and cathode interface displayed different thickness. To be precise, the IMC layer thickness formed at the cathode interface was larger than that of formed at the anode interface, which was contradictory with the traditional theory of EM effect on IMC growth in SnAgCu or SnAg solder joints. By calculation, the cathodic scallop-type IMC thickness can reach 34.3μm, however, merely 9.7μm-thick IMC layer was found at the anode interface. It should be noticed that a uniform 7.5μm-thick Bi layer was aggregated between the IMC layer and the solder matrix at the anode interface. The diffusion and migration path of the Sn atoms to the anode interface was blocked because of the compact Bi layer formation, which reduced the actual Sn reacted with Cu to form IMC. Accordingly, the growth rate of the IMC layer decreased, leading to the abnormal IMC growth at the interfaces. © 2013 IEEE.

Keyword:

Silver alloys Morphology Growth kinetics Lead-free solders Anodes Copper Copper alloys Electromigration Tin alloys Growth rate Packaging materials Soldered joints Tin Microstructure Cathodes

Author Community:

  • [ 1 ] [He, Hongwen]National Center of Advanced Package China, Building D1, Sensor Network International Science Park, Wuxi, Jiangsu, 214315, China
  • [ 2 ] [Cao, Liqiang]National Center of Advanced Package China, Building D1, Sensor Network International Science Park, Wuxi, Jiangsu, 214315, China
  • [ 3 ] [Hao, Hu]National Center of Advanced Package China, Building D1, Sensor Network International Science Park, Wuxi, Jiangsu, 214315, China
  • [ 4 ] [Xu, Guangchen]College of Materials Science and Engineering, Beijing University of Technology, Beijing, 100124, China
  • [ 5 ] [Ma, Limin]College of Materials Science and Engineering, Beijing University of Technology, Beijing, 100124, China
  • [ 6 ] [Guo, Fu]College of Materials Science and Engineering, Beijing University of Technology, Beijing, 100124, China

Reprint Author's Address:

Email:

Show more details

Related Keywords:

Related Article:

Source :

ISSN: 1550-5723

Year: 2013

Page: 223-229

Language: English

Cited Count:

WoS CC Cited Count: 0

SCOPUS Cited Count: 1

ESI Highly Cited Papers on the List: 0 Unfold All

WanFang Cited Count:

Chinese Cited Count:

30 Days PV: 6

Online/Total:700/10578851
Address:BJUT Library(100 Pingleyuan,Chaoyang District,Beijing 100124, China Post Code:100124) Contact Us:010-67392185
Copyright:BJUT Library Technical Support:Beijing Aegean Software Co., Ltd.