Abstract:
GdB6 and CeB6 were used as raw materials, and hexaborides GdxCe1-xB6 (x=0.0 similar to 1.0) bulk materials were prepared by spark plasma sintering (SPS). The effects of Gd doping on the phase composition, the mechanical properties, the resistivity and the thermionic emission properties of the CeB6 base material were studied. The results show that high density GdxCe1-xB6 single-phase block material can be obtained with the sintering parameters including the temperature 1550 degrees C, the pressure 50 MPa and holding time 5 min. And the Vickers hardness of the sintered samples can reach 24.02 GPa. The thermionic emission properties results show that the proper amount of Gd doping can significantly improve the electron emission properties of bulk materials. Gd0.1Ce0.9B6 composition block has the best thermal emission properties; its emission current density is 101.57 A/cm(2), the zero field current density is 21.94 A/cm(2), and the average effective work function is 2.34 eV under the applied voltage condition of 4 kV at 1600 degrees C, which are better than those of GdB6 and CeB6 block samples under the same conditions.
Keyword:
Reprint Author's Address:
Email:
Source :
RARE METAL MATERIALS AND ENGINEERING
ISSN: 1002-185X
Year: 2016
Issue: 12
Volume: 45
Page: 3267-3270
0 . 7 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
ESI HC Threshold:305
CAS Journal Grade:4
Cited Count:
WoS CC Cited Count: 3
SCOPUS Cited Count:
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 8
Affiliated Colleges: