Indexed by:
Abstract:
分别以Ce_2(C_2O_4)_3和Ce(SO4)2为Ce前驱体,采用固相球磨法制备了Ce基选择性催化还原(SCR)脱硝催化剂CeTiO_x-A[以Ce_2(C_2O_4)_3为前驱体]和CeTiO_x-B[以Ce(SO4)2为前驱体].将2个催化剂分别在体积分数为0. 15%的SO2的气氛下反应40和60 h,得到高硫条件下SCR反应后的CeTiO_x催化剂,分别记为40CeTiOx-A,60CeTiOx-A,40CeTiOx-B和60CeTiOx-B.考察了反应前后催化剂的NH_3-SCR反应活性.采用X射线衍射(XRD)、X射线荧光光谱(XRF)、比表面积(BET)测试、H2程序升温还原...