通过改性Pechini方法合成不同Co含量的富锂正极材料Li[Li(1/3-x/3)CoxMn(2/3-2x/3)]O2(x=0.4,0.5,0.6).XRD研究结果表明,不同Co含量的富锂正极材料均具有良好的层状结构,结晶度高.电化学测试结果表明材料的初始容量随Co含量的增加而增加,在200~220 mAh/g之间.其中x=0.4材料的循环性能最佳,在0.5 C(100 mA/g)时,循环50次后的容量保持率为75%.容量微分曲线研究结果表明在3.5 V以下出现了Mn4+/Mn3+的还原峰,并随循环次数的增加峰面积加大.循环过程的XRD研究表明,随着充放电次数的增加,富锂正极材料的层状结构逐渐向尖晶石相转变,且有杂质相MOx(M=Co,Mn)生成,导致容量衰减.