The interfacial morphology and corrosion resistance of low carbon Fe-B cast steels in zinc bath at 520 degrees C were investigated. The results show Fe-B cast steel containing high Cr and Ni exhibits the best corrosion resistance to liquid zinc. The corrosion layers are composed of Gamma-Fe3Zn10, delta-FeZn10, xi-FeZn13 and eta-Zn. The corrosion behaviour of Fe-B cast steels includes the following processes: the preferential leach and dissolution of Cr and Ni, the formation of Fe-Zn compounds controlled by zinc atom diffusion, and the spalling of borides without the supporting role of alpha-(Fe, Cr) matrix corroded by liquid zinc. Crown Copyright (C) 2011 Published by Elsevier Ltd. All rights reserved.
Keyword:
Reprint Author's Address:
Source :
CORROSION SCIENCE
ISSN: 0010-938X
Year: 2011
Issue: 9
Volume: 53
Page: 2826-2834
8 . 3 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
JCR Journal Grade:1
CAS Journal Grade:1
Cited Count:
WoS CC Cited Count: 68
SCOPUS Cited Count: 74
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 5
Affiliated Colleges: