用紧凑拉伸(CT)试件,测试了API 5L X52管材及焊管接头的疲劳裂纹扩展速率,根据泵站的载荷谱,估算了管线的服役寿命.指出管线运行载荷谱及焊管缺陷对石油管线的服役寿命有重要影响.减少运行中管线的压力波动、消除焊趾缺陷、严格焊管生产的无损检查,对延长管线的服役寿命有重要作用.