Abstract:
一种提高富硼渣活性的方法,属于矿物利用技术领域。先将富硼渣破碎至10~40目,然后将60~80目的TiO2和ZrO2加入到上述富硼渣中,并在搅拌机中搅拌15~20分钟,使TiO2和ZrO2与富硼渣混合均匀,最后将上述含TiO2和ZrO2的富硼渣随炉加热至1510~1550℃,保温2~3小时,以80~100℃/小时的冷却速度冷却至温度低于850℃后,出炉空冷至室温,即可得到活性高的富硼渣产品。