This paper focused on toughening mechanism of weld metal for self-shielded flux-cored wire after a review of development history of self-shielded flux-cored wire. Toughness impact of inclusion depended on its shape and sizes. Circular inclusion ranging from 0.2 to 1.0μm has a tendency to form AF core and is favorable for toughness improvement. To maintain the relatively higher toughness, optimum ratio of aluminum to oxygen in weld metal is 0.84. The additions of trace element such as Li, Zr, Ti, B, Ni and Ce in flux-cored wire help to improve weld impact toughness. In addition, droplet transfer modes and formation mechanism of spatter was also summarized.

Keyword:

Droplet transfer; Self-shielded flux-cored wire; Spatter; Toughening mechanism

Author Community:

  • [ 1 ] [Song, S.]Beijing University of Technology, Beijing 100124, China
  • [ 2 ] [Li, Z.]Beijing University of Technology, Beijing 100124, China
  • [ 3 ] [Li, G.]Beijing University of Technology, Beijing 100124, China

Reprint Author's Address:

  • [Song, S.]Beijing University of Technology, Beijing 100124, China

Email:

Show more details

Related Keywords:

Related Article:

Source :

China Mechanical Engineering

ISSN: 1004-132X

Year: 2010

Issue: 14

Volume: 21

Page: 1752-1757

Cited Count:

WoS CC Cited Count: 0

SCOPUS Cited Count:

ESI Highly Cited Papers on the List: 0 Unfold All

WanFang Cited Count:

Chinese Cited Count:

30 Days PV: 1

Online/Total:926/10619325
Address:BJUT Library(100 Pingleyuan,Chaoyang District,Beijing 100124, China Post Code:100124) Contact Us:010-67392185
Copyright:BJUT Library Technical Support:Beijing Aegean Software Co., Ltd.