Abstract:
Textured Ca3Co4O9 ceramics were successfully prepared by combination oxalate coprecipitation method and spark plasma sintering (SPS) technique. Single-phase Ca3Co4O9 ceramics with grain aligned can be obtained by spark plasma sintering at 30 MPa, 850 degrees C for 5 min using the coprecipitation precursor powders calcined at 800 degrees C for 6 or 8h. The SPS process is effective sintering technology to obtain pure phase and textured Ca3Co4O9 Ceramics. During SPS treatment the densification and reaction occur simultaneously. The thermoelectric properties of the prepared ceramics sample were investigated from 100 to 700 degrees C. At 700 degrees C, the electrical resistivity, Seebeck coefficient, thermal conductivity and ZT of the sample prepared by the powders calcined at 800 degrees C for 8h are 7.50 x 10(-5) Omega m, 165 mu VK-1, 1.62 W m(-1) K-1, and 0.22, respectively. (C) 2008 Elsevier B.V. All rights reserved.
Keyword:
Reprint Author's Address:
Email:
Source :
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY
ISSN: 0924-0136
Year: 2008
Issue: 1-3
Volume: 208
Page: 70-74
6 . 3 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
JCR Journal Grade:2
Cited Count:
WoS CC Cited Count: 48
SCOPUS Cited Count: 55
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 4
Affiliated Colleges: