Indexed by:
Abstract:
Sub-micrometer Sc2O3-W powder with a narrow particle size distribution has been obtained by a sol-gel method combined with two-step hydrogen reduction process. Based on the obtained powder, the W-Sc2O3 targets have been sintered via spark plasma sintering (SPS) at 1300 degrees C. The W-Sc2O3 targets have the average grain size of about 1 pm. Both the sintering temperature and holding time are much lower than those of the targets prepared with micrometer sized powders. The obtained W-Sc2O3 targets have a high comparative density of 96.4% and rockwell hardness of 86.4 HRC. Using the target, the scandate cathode deposited with a film containing 5% Sc2O3 and 95% W has been obtained by pulsed laser deposition (PLD) method. This cathode has good emission property, i.e., the highest thermionic emission current density reaches 43.09 A/cm(2) of idly at 900 Cb after being activated for 8 h, which is much higher than that of scandate cathode without film. Scandium (Sc) supplied by the film on the surface during the activation forms a Ba-Sc-O active layer, which helps to the emission. (C) 2013 Elsevier Ltd. All rights reserved.
Keyword:
Reprint Author's Address:
Email:
Source :
MATERIALS RESEARCH BULLETIN
ISSN: 0025-5408
Year: 2013
Issue: 12
Volume: 48
Page: 5040-5044
5 . 4 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
JCR Journal Grade:2
CAS Journal Grade:3
Cited Count:
WoS CC Cited Count: 10
SCOPUS Cited Count: 11
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 6
Affiliated Colleges: