Indexed by:
Abstract:
Sn-37Pb and Sn-3.0Ag-0.5Cu solder pastes printed onto a board were attached to ball grid array (BGA) samples using Sn-3.0Ag-0.5Cu solder balls. Before thermal shock, the initial grain orientations on the cross-section were obtained by scanning electron microscopy equipped with an electron backscattered diffraction system. Three mixed solder joints (two from the corner and another from the middle of the BGA component) and three lead-free solder joints (at the same positions) were selected to investigate the recrystallization behavior under thermal shock (TS) cycling conditions. All of the mixed and lead-free solder joints were initially single crystal. The results showed that recrystallization occurred in both the mixed and lead-free solder joints after 200 TS. For the mixed solder joints, more recrystallization was observed and the location of samples had a significant influence on their recrystallization behavior, while location was not as important for the lead-free samples after 200 TS in this study. Both the mixed and lead-free solder joints at the corner of BGA components showed the poorest reliability. According to misorientation distribution maps and subgrain rotation behaviors, the reliability of mixed solder joints was much poorer than that of lead-free solder joints.
Keyword:
Reprint Author's Address:
Email:
Source :
JOURNAL OF ELECTRONIC MATERIALS
ISSN: 0361-5235
Year: 2018
Issue: 7
Volume: 47
Page: 4156-4164
2 . 1 0 0
JCR@2022
ESI Discipline: MATERIALS SCIENCE;
ESI HC Threshold:260
JCR Journal Grade:3
Cited Count:
WoS CC Cited Count: 15
SCOPUS Cited Count: 14
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 8
Affiliated Colleges: