以WF6、H2为原料,采用化学气相沉积法沉积制备出不同直径难熔金属钨管。对不同沉积温度(500℃,600℃,700℃)沉积制备钨管的纯度、密度、显微硬度、残余应力及钨管强度进行了测试与分析研究。研究结果表明:沉积制备钨管具有高纯度和高致密度;随着沉积温度、钨管半径(3~20 mm)不同,显微硬度值在500~800 HV之间;沿钨管圆周、半径方向存在较大残余应力;抗拉强度范围在300~500 MPa.